Home › Mining › Barkly Rare Earths (ASX:BAK)

Barkly Rare Earths adds a second high-extraction processing route

Mining By Maxwell Dee 3 min read

Barkly Rare Earths has recorded 97% to 98% magnet rare earth oxide extraction in three dry-calcination and acid-leach tests. The result gives the ASX explorer two high-extraction processing routes, although scale-up, downstream recovery and economics remain unresolved.

  • 97% to 98% MREO extraction across three sighter tests
  • Dry calcination used no acid or other reagents
  • Only 8% to 10% of calcined mass dissolved
  • 97% to 99% phosphorus extraction creates a possible by-product opportunity
  • Larger-scale testing and flowsheet comparison are next

Dry calcination delivers high rare earth extraction

Barkly Rare Earths Limited (ASX:BAK) has produced a second high-extraction processing result at its Barkly Project, with dry calcination followed by acid leaching recovering 97% to 98% of magnet rare earth oxides in three independent sighter tests.

The work, completed by Nagrom on a composite sample, used thermal treatment at 600°C and 700°C without adding acid or other reagents during calcination. Sulphuric acid leaching recovered 97% of MREO at both temperatures, while a hydrochloric acid test on the 700°C calcine reached 98%.

The result builds on the company’s earlier 99% extraction test and gives Barkly two routes that have now extracted at least 97% of MREO to the acid leach solution: calcination and acid leaching, and caustic conversion followed by acid leaching. The comparison remains indicative because the test conditions differed between the programmes.

Selective dissolution could simplify the flowsheet

Only 8% to 10% of the calcined sample mass dissolved during leaching, while the MREO-bearing material largely reported to the solution. Residue grades were 19 to 39 parts per million MREO, compared with calculated leach head grades of 1,110 to 1,120 parts per million.

That selective dissolution is potentially important for plant design, but it is not yet a demonstrated cost advantage. Barkly says avoiding reagents during the thermal stage could reduce acid handling, off-gas scrubbing and associated operating complexity compared with a caustic conversion flowsheet. Capital intensity, energy consumption, acid requirements and impurity management still need to be assessed side by side.

Phosphorus recovery remains an untested opportunity

Phosphorus extraction was also high, at 97% to 99% across the three tests, while yttrium extraction reached 90% in each test. Barkly says the phosphorus co-dissolution is consistent with the project’s rare earths being hosted in aluminium-phosphate-sulphate minerals and may support a future by-product stream.

That possibility has not yet been tested. The next programme is intended to repeat the work on larger, more representative composites, optimise grind size, calcination temperature and residence time, and examine impurity removal, rare earth product recovery and phosphorus separation. Downstream recovery of a saleable rare earth product has not been demonstrated.

Scale-up will determine whether the result matters economically

The current tests used a small composite representing selected drilling intervals, so the company cautions that the results cannot be extrapolated across the project. The three leach tests also used different acids, temperatures and residence times, meaning the performance difference cannot be attributed to acid type alone. Barkly is also progressing physical beneficiation work to assess whether flotation can upgrade the rare earths and reject gangue before leaching.

The company’s work programme includes continuing Phase 1 drilling assays, a Mineral Resource update targeted for the fourth quarter of 2026 and further resource and Exploration Target updates in the first quarter of 2027. The immediate technical question is whether the extraction rates survive a larger and more representative test, while the commercial question is whether a simpler flowsheet can offset the energy and reagent demands of thermal treatment.

Bottom Line?

Barkly now has two promising high-extraction routes, but the investment case still depends on scale-up, product recovery and a credible comparison of energy and processing costs.

Questions in the middle?

  • Will the 97% to 98% MREO extraction rates hold when larger, representative composites are tested?
  • Can Barkly recover a saleable rare earth product while managing phosphorus and other impurities?
  • Will dry calcination prove cheaper overall than caustic conversion once energy, acid and plant requirements are included?

Sources